Tapered roller bearings are separable bearings, bearing inner and outer rings with tapered raceways line. These bearings are mounted on roller rows into single row, double row and four row tapered roller bearings, such as different structural types. Single row tapered roller bearings can bear radial load and axial load in one direction. When the bearing radial load
2013年9月26日星期四
live rolling raceway surface stripping
NTN Precision bearing damage and countermeasures
NTN Bearing the correct use , it can have a long life. If damage occurs prematurely , probably because selection errors, improper use or poor lubrication . Therefore, NTN bearings installed , we need to record the machine type, installation location, conditions of use and its surrounding complex , bearing damage through the study concluded the type of problem occurs when the use of the environment , in order to prevent the situation from happening again.
Bearing operation can not be observed directly , but through the noise , vibration , temperature, Backing bearings lubricant known abnormal status . The following are common injuries and NTN Bearing countermeasures.
1 Peel : live rolling raceway surface stripping , stripping was uneven .
Cause: The load is too large , the use of bad ; poor installation ; shaft or bearing housing precision bad ; games is not enough ; dust into ; rust ; improper lubrication ; temperature rise in the case of lower hardness .
Action: Re-select bearings ; reconsider clearance inspection shaft and bearing housing precision ; re-examine the conditions of use ; Check the installation method ; checking lubricants and lubrication methods .
2 Burn : bearing severe temperature rise , resulting in burns, can not rotate.
Cause: The clearance is too small ; lack of lubrication or improper lubricant ; roller tilt ; overload ; in the case of temperature rise , lower hardness .
Action: Check the type of lubricant and make sure that the amount of fill ; setting the appropriate clearance ; check the conditions of use ; prevent bearing centerline tilt ; checking around the bearing design ;
3 cage damage : rivets loose or broken , cage rupture.
Cause: The torque load is too large ; frequent changes in speed or high-speed rotation ; poor lubrication ; snaps into foreign body ; vibration ; poor installation .
Action: Check lubrication conditions ; re-examine the choice of the cage ; check the conditions of use ; improved installation method.
4 abrasion : There are two abrasive types, one , red wear particles generated with the surface , first , in the rolling body produces Brinell
Reason: lack of interference ; bearing swivel inadequate ; insufficient lubrication ; variable load , charge stability vibration
Action: Check the state interference and lubricants segment ; transportation inside and outside the ring packaged separately ; reselect lubricant ; bearing reselected.